TEST
TECHNICAL
STANDARD
REFERENCE
UNIT
REQUIREMENT
RESULT
UPPER
Impact
abrasion
resistance
EN
13634:2017
Section
4.4.4
seconds
Area A: (Achilles’ and instep)
Level 1: ≥ 1.5 s
Level 2: ≥ 2.5 s
Level 1
Area B: (Remainder of boot upper)
Level 1: ≥ 5 s
Level 2: ≥ 12 s
Upper is classified based on the lowest result obtained in either area A or B
For a definition of Area A and B see Fig. 2 and Chart 3
Impact cut
resistance
EN
13634:2017
Section
4.4.5
mm
Area A: (Achilles’ and instep)
Level 1: ≤ 25 mm maximum knife penetration
Level 2: ≤ 25 mm maximum knife penetration
Level 1
Area B: (Remainder of boot upper)
Level 1: ≤ 25 mm maximum knife penetration
Level 2: ≤ 15 mm maximum knife penetration
Upper is classified based on the lowest result obtained in either area A or B
For a definition of Area A and B see Fig. 2 and Chart 3
CHART 2:
CARGA CE
BOOTS TYPE EXAMINATION TEST RESULTS ACCORDING TO
EN 13634:2017
(CONT.)
TEST
TECHNICAL
STANDARD
REFERENCE
UNIT
REQUIREMENT
RESULT
SOLE
Transverse rigidity
of footwear
EN
13634:2017
Section
4.8
kN
Level 1: ≥ 1.0 kN
Level 1
Level 2: ≥ 1.5 kN
BOOT
Slip resistance
of sole
EN
13634:2017
Section
5.4
Surface: ceramic - Lubricant: SLS solution
A) heel mode (7°) ≥ .28
B) flat mode ≥ .32
SRA
CHART 2:
CARGA CE
BOOTS TYPE EXAMINATION TEST RESULTS ACCORDING TO
EN 13634:2017
(CONT.)
2021-03-17_CargaCEBootManual.indd 10-11
2021-03-17_CargaCEBootManual.indd 10-11
3/18/21 4:34 PM
3/18/21 4:34 PM