32
Operating manual
NEOPULSE 400 CW
Translation of the original
instructions
WELDING PROCESSES
For more information on GYS pre-installed user settings and welding processes, scan the QR code:
SPOT WELDING MODE
• SPOT WELDING
This welding mode allows the pre-assembly of parts before welding. Spot welding can be done manually using the trigger or timed with a predefined
spot welding period. This spot welding makes reproduction and execution of non-oxidised weld points easier (accessible in the advanced menu).
• TIME LIMITS
This is a welding mode similar to SPOT welding but with predefined weld and dwell times, as long as the trigger is held down.
CONFIGURING THE SETTINGS
Units
Wire speed
m/min
Amount of filler metal deposited and consequently the welding intensity and penetration.
Voltage
V
Control over the cord’s width.
Self
-
Lessens the welding current more or less. To be set according to the welding position.
Pre-Gas
s
When the torch is bled and the gas shield is created before ignition.
Post-Gas
s
Duration of the gas protection after the arc is extinguished. It protects the workpiece and the electrode from
oxidation.
Thickness
mm
The pre-installed user settings (syngergies) allow for a fully-automatic set-up. Working with different
thicknesses
automatically sets the appropriate thread tension and speed.
Start-up
A
The welding current is set according to the type of wire used and the material to be
welded.
Arc length
-
Used to adjust the distance between the end of the wire and the weld pool (tension adjustment).
Approach speed
%
Progressive yarn speed. Before priming, the wire moves slowly to create the first contact without jolting.
Hot Start
% & s The Hot Start is an overcurrent used at the start that prevents the wire from sticking to the workpiece. The
intensity (% of welding current) and the time (seconds) can be programmed.
Crater Filler
%
This idling bearing current is a phase after the current is lowered.
The intensity (% of welding current) and the time (seconds) can be programmed.
Soft Start
s
Gradual current increase. The current is controlled between the first contact and the welding process in order
to avoid the possibility of violent ignitions or jolts.
Uplsope
s
Upslope current
Cold current
%
Second welding current known as a «cold» welding current.
Pulse frequency
Hz
Pulse frequency
Duty cycle
%
In pulsed mode, the hot current time is adjusted in relation to the cold current time.
Downslope
s
Downslope current.
Tack welding
s
Set duration.
Time between two
points
s
Time between the end of a point (excluding Post-Gas) and the start of a new point (including Pre-Gas).
Burnback
s
Feature preventing the thread sticking to the bead. This is timed to coincide with the wire rising from the weld
pool.
Access to some welding settings depends on the welding process (Manual, Standard, etc.) and the selected display mode (Easy, Expert or Ad-
vanced). Refer to the HMI manual.
Содержание NEOPULSE 400 CW
Страница 3: ...FR 3 Manuel d utilisation NEOPULSE 400 CW Notice originale Chaine Chain M4x10 x6...
Страница 140: ...RU 20 HMI NEOPULSE 220 C NEOPULSE 220 C XL NEOPULSE 320 C NEOFEED 4W NEOPULSE 400 CW 1 86 MMI...
Страница 141: ...21 4 8 7 1 2 6 5 3 1 2 n 1 3 n 2 4 5 n 3 6 n 4 Job 7 8 1 2 3 1 2 3...
Страница 143: ...23 AM PM AUTO 10 1 4 0000...
Страница 144: ...RU 24 jobs 2 X n 3 n 3 10 0000 I 0 0A 0 A 50A U 0 0V 0 1V 5 0V 0 0 0 1 5 0 Admin n 4 OFF ON 4 0000 3 6 314159...
Страница 146: ...RU 26 USB USB USB Job Jobs Removable disk Portability USB Job USB Job USB USB...
Страница 149: ...29 Warning CR2032...