Design and function
Transport and installation
44
099-004968-EW501
13.09.2021
5.1.11.5 Spot welding
Figure 5-16
1. Start
• Press and hold torch trigger.
• Shielding gas is expelled (gas pre-flows).
• Wire feed motor runs at "creep speed".
• Arc ignites after
the wire electrode makes contact with the workpiece; welding current flows.
• Changeover to the pre-selected wire speed after the set ignition time (tZn).
• The WF stops after the set spot welding time elapses.
• Arc is extinguished after the pre-selected wire burn-back time elapses.
• Gas post-flow time elapses.
2. End
• Release torch trigger.
When the torch trigger is released, the welding process is also interrupted even before the spot
time elapses. With fast tacking (time between two welding process under approx. 1.5 seconds) the
gas pre-flow, the creep process and also the ignition time (tZn) are not required.