SERVICE MANUAL
180
OPERATION 6-8 0-5461
FAULT
CAUSE
REMEDY
9 Arc start is not smooth.
A Tungsten electrode
is too large for the
welding current.
A Select the right size tungsten electrode.
Refer to Table 6-1 Cigweld Tungsten
Electrode Selection Chart.
B The wrong electrode
is being used for the
welding job.
B Select the right size tungsten electrode
type. Refer to Table 6-3 Cigweld Tungsten
Electrode Selection Chart.
C Shielding gas flow rate
is too high.
C Select the right shielding gas flow rate
for the welding job. Refer to Table 6-5 on
page 6-7
D Incorrect shielding gas
is being used.
D Select the correct shielding gas.
E Poor work clamp
connection to work
piece.
E Improve connection to work piece.
10 Arc flutters during TIG
welding.
Tungsten electrode
is too large for the
welding current.
Select the right size tungsten electrode.
Refer to Table 6-1 Cigweld Tungsten
Electrode Selection Chart.
Table 6-6: GTAW (TIG) Welding Problems
Содержание WELDSKILL 180
Страница 20: ...SERVICE MANUAL 180 INTRODUCTION 2 8 0 5461 This Page Intentionally Blank ...
Страница 24: ...SERVICE MANUAL 180 INSTALLATION 3 4 0 5461 This Page Intentionally Blank ...
Страница 28: ...SERVICE MANUAL 180 OPERATION 4 4 0 5461 This Page Intentionally Blank ...
Страница 54: ...SERVICE MANUAL 180 ROUTINE SERVICE REQUIREMENTS 7 4 0 5461 This Page Intentionally Blank ...
Страница 56: ...THEORY OF OPERATION 8 2 0 5461 SERVICE MANUAL 180 This Page Intentionally Blank ...
Страница 64: ...PRELIMINARY TROUBLESHOOTING POWER SOURCE 10 6 0 5461 SERVICE MANUAL 180 This Page Intentionally Blank ...
Страница 76: ...KEY SPARE PARTS 13 2 Manual 0 5461 SERVICE MANUAL 180 This Page Intentionally Blank ...
Страница 79: ...SERVICE MANUAL 180 This Page Intentionally Blank ...