3.6 Tungsten electrode selection
Base metal type
Thickness
range
Desired results
Welding
current
Electrode type
Shielding gas Tungsten performance characteristics
Copper alloys,
Cu-NI alloys and
Nickel alloys
All
General purpose DCSP
2% Thoriated
(EW-Th2)
75% Argon/
25% Helium
Best stability at medium currents. Good arc
starts
Medium tendency to spit
Medium erosion rate
2% Ceriated
(EW-Ce2)
75% Argon/
25% Helium
Low erosion rate. Wide current range. AC or
DC. No spitting. Consistent arc starts
Good stability
Only thick
sections
Increase
penetration or
travel speed
DCSP
2% Ceriated
(EW-Ce2)
75% Argon/
25% Helium
Low erosion rate. Wide current range. AC or
DC. No spitting. Consistent arc starts
Good stability
Mild Steels,
Carbon Steels,
Alloy Steels,
Stainless Steels
and Titanium
alloys
All
General purpose DCSP
2% Thoriated
(EW-Th2)
75% Argon/
25% Helium
Best stability at medium currents. Good arc
starts
Medium tendency to spit
Medium erosion rate
2% Ceriated
(EW-Ce2)
75% Argon/
25% Helium
Low erosion rate. Wide current range. AC or
DC. No spitting Consistent arc starts
Good stability
2% Lanthanated
(EWG-La2)
75% Argon/
25% Helium
Lowest erosion rate. Widest current range on
DC. No spitting. Best DC arc starts and stability
Only thick
sections
Increase
penetration or
travel speed
DCSP
2% Ceriated
(EW-Ce2)
75% Argon/
25% Helium
Low erosion rate. Wide current range. No
spitting. Consistent arc starts. Good stability
2% Lanthanated
(EWG-La2)
Helium
Lowest erosion rate. Highest current range. No
spitting. Best DC arc starts and stability
19
BOC Smootharc 180 Multiprocess operating manual
Summary of Contents for 180 Multiprocess
Page 1: ...180 Multiprocess Operating manual 6PRRWKDUF GYDQF GYDQF ...
Page 45: ...45 BOC Smootharc 180 Multiprocess operating manual ...
Page 53: ......
Page 54: ......
Page 55: ......