7
2.4
Paste the Masking Tape
Tear the broken tape and paste a new one, pay attention not to overlap and too large clearance.(If the tape
is not broken, it can be reused).
2.5
Install the Material (for example, PLA materials)
1.
Click Control Panel from “Unload” to “ head preheat”, adjust the extrusion nozzle temperature to 205°C. Turn “ON” ( left), extrusion
nozzle temperature is automatically heated to 205°C.
2.
Insert the material
3.
When the temperature rises to 205°C, press the material at the entrance of shrapnel, insert the material, the material squeezing
down, if the material is melted and flow out from nozzle, and the material is inserted successfully.