CABLINE-VS II PLUG Assembly Manual
Document No.
ASM-17005
8
/
16
Confidential C
⑤
Center-conductors are soldered with pulse heater. See photo.3 of soldering condition.
Photo.3 AWG#40
Caution: The SHELL bottom side of PLUG HSG ASS'Y has convex shape at the points shown in Fig.4, so please make escape shape on
the receiving jig of the pulse heater to prevent interference.
Fig.4 The SHELL bottom side of PLUG HSG ASS'Y
※
When solder bridge is appeared between the terminal, try heating again with pulse heater only one time.
If the bridge isn’t repaired, use the soldering iron only a NG point.
Condition of Soldering iron
:
50W
Operating temperature
:
350
℃
Application time of soldering iron
:
Within 5sec.
※
Because it might give product damage, please do not instigate a cable after soldering.
※