12-14. Troubleshooting
−
Waviness Of Bead
Waviness Of Bead
−
weld metal that is not parallel and does not cover
joint formed by base metal.
S-0641
Possible Causes
Corrective Actions
Welding wire extends too far out of nozzle.
Be sure welding wire extends not more than 1/2 in. (13 mm) beyond nozzle.
Unsteady hand.
Support hand on solid surface or use two hands.
12-15. Troubleshooting
−
Distortion
Distortion
−
contraction of weld metal during welding that forces
base metal to move.
Base metal moves
in the direction of
the weld bead.
S-0642
Possible Causes
Corrective Actions
Excessive heat input.
Use restraint (clamp) to hold base metal in position.
Make tack welds along joint before starting welding operation.
Select lower voltage range and/or reduce wire feed speed.
Increase travel speed.
Weld in small segments and allow cooling between welds.
Notes
Summary of Contents for Multi-Handler 200
Page 42: ... A complete Parts List is available at www HobartWelders com OM 285922 Page 39 Ref 287984 B ...
Page 43: ...OM 285922 Page 40 7 2 Welding Parameters 240 Volt Ref 287984 B ...
Page 44: ... A complete Parts List is available at www HobartWelders com OM 285922 Page 41 Ref 287984 B ...
Page 50: ...OM 285922 Page 47 Notes ...
Page 51: ...OM 285922 Page 48 SECTION 9 ELECTRICAL DIAGRAM Figure 9 1 Circuit Diagram ...
Page 52: ...OM 285922 Page 49 287757 A ...
Page 74: ...Notes ...