Design and function
TIG welding
099-005545-EW501
17.12.2020
43
5.3.4.1 Hotstart settings
The setting ranges for the parameter values are summarised in the Parameter overview sec-
tion
> see 11.2 chapter
.
• Select MMA JOB 128
> see 5.3.2 chapter
.
2s
2s
Figure 5-28
Display
Setting/selection
Hotstart current
Hotstart time
5.3.5 Antistick
The Antistick feature prevents the electrode from annealing.
Should the electrode stick despite the Arcforce feature, the machine au-
tomatically switches to the minimum current within approx. one second.
This prevents the electrode from annealing. Check the welding current
setting and correct for the welding task in hand.
Figure 5-29
5.4 TIG welding
5.4.1 Preparing the TIG welding torch
The TIG welding torch is to be equipped to suit the relevant welding task!
• Fit suitable tungsten electrodes and
• an appropriate shielding gas nozzle.
• Observe the operating instructions for the TIG welding torch!