Thick, dimpled finish "orange
Gun too close to surface.
Check distance. Normally approx. 8".
peel".
Too much material coarsely atomized.
Increase air pressure or decrease fluid pressure.
Air pressure too low.
Increase air pressure or reduce fluid pressure.
Improper thinner being used.
Follow paint manufacturer's mixing instructions.
Material not properly mixed.
Follow paint manufacturer's mixing instructions.
Surface rough, oily, dirty.
Properly clean and prepare.