background image

When attached to either a PosiTector Standard or Advanced body, the 

PosiTector 

6000

FNDS

probe measures the individual thicknesses of both the paint and the zinc layers

in a duplex coating system with a single reading.

Duplex coating systems use a combination of two corrosion protection systems –
typically paint or powder coating over galvanized steel (hot-dip, electro or zinc spray
metallizing). The resultant corrosion protection is superior to either protection system
used independently.

Duplex Mode

In Duplex mode, the Gage utilizes both magnetic (ferrous) and eddy current (non-
ferrous) principles simultaneously to calculate and display the individual paint and zinc
layer thicknesses.  The magnetic principle is used to measure the combined paint/zinc
thickness over the ferrous substrate and the eddy current principle is used to measure
the paint thickness over the non-ferrous zinc coating. The zinc thickness is calculated
by subtracting the paint thickness from the combined paint/zinc thickness
measurement.

PosiTector

®

6000 FNDS

probe

for Duplex Coatings

Addendum to Instruction Manual v. 7

Summary of Contents for PosiTector 6000 FNDS

Page 1: ...ither protection system used independently Duplex Mode In Duplex mode the Gage utilizes both magnetic ferrous and eddy current non ferrous principles simultaneously to calculate and display the individual paint and zinc layer thicknesses The magnetic principle is used to measure the combined paint zinc thickness over the ferrous substrate and the eddy current principle is used to measure the paint...

Page 2: ...AT LEAST 2 inches 5 cm between readings or leave the probe on the surface in the same location for continuous measurements Verify accuracy on reference standards at the beginning and the end of each shift or if the gage is dropped or suspected of giving erroneous readings When enabled default the Gage will display two measurement values as shown above To disable uncheck Duplex within the Setup Men...

Page 3: ...nt 1 Select F Zero from the Cal Settings menu 2 Press to select the number of readings to be used to obtain an average typically 3 to 10 readings The greater the variation between readings the more zero readings should be taken to obtain an average 3 Repeatedly measure the uncoated steel part The Gage will wait two seconds after placing the probe on the surface to allow the user to correctly posit...

Page 4: ...o correctly position the probe on the surface After the last measurement the Gage will calculate and display the reading which represents the average of all the measurements taken If the expected reading is not obtained within tolerance lift the probe from the surface and adjust the reading down or up to the expected thickness and press NOTE The reference thickness should be similar to the expecte...

Reviews: