Troubleshooting – MIG Weld Quality
Fault
Cause
Remedy
Cold weld puddle
Loose welding cable connection.
Check
all
welding
cable
connections
Low power supply voltage.
Contact supply authority
Arc does not have a crisp
sound that short arc
exhibits when the wire feed
speed and voltage are
adjusted correctly
The MIG torch has been connected
to the wrong voltage polarity on the
front panel.
Connect the MIG torch to the
positive (+) welding terminal for
solid wires and negative (-)
welding terminal for gasless
wires.
Refer to the wire manufacturer
for the correct polarity.
Table 14
Содержание WeldForce WF-205MST
Страница 36: ... 36 Weldclass 2019 E O E Edition 2 1 Figure 25 ...
Страница 37: ...WF 205MST Weldclass 2019 E O E Edition 2 1 37 8 6 Primary Schematic Circuit Diagram Figure 26 ...
Страница 42: ... 42 Weldclass 2019 E O E Edition 2 1 Figure 33 Figure 34 Figure 35 Figure 36 ...
Страница 77: ...WF 205MST Weldclass 2019 E O E Edition 2 1 77 NOTES ...
Страница 78: ... 78 Weldclass 2019 E O E Edition 2 1 ...
Страница 79: ...WF 205MST Weldclass 2019 E O E Edition 2 1 79 ...
Страница 80: ... 80 Weldclass 2019 E O E Edition 2 1 www Weldclass com au WF 205MST ...