![FIBER FOX Mini 22A Скачать руководство пользователя страница 28](http://html1.mh-extra.com/html/fiber-fox/mini-22a/mini-22a_user-manual_2286588028.webp)
- 28 -
Note
: A vertical line sometimes appears at the splice point when MM fibers, or dissimilar fibers (different diam-
eters) are spliced. This does not affect splice quality, such as splice loss or tensile strength.
Fat
Fiber stuffing too much
Decrease [Overlap] and
perform [Motor calibration]
Thin
Arc power not adequate
Perform [Arc calibration]
Some arc parameters not
adequate
Adjust [Prefuse power],
[Pre-fuse time] or [Overlap]
Line
Some arc parameters not
adequate
Adjust [Prefuse power],
[Pre-fuse time] or [Overlap]