While it is important to note the average of several readings, it is even more important to 
note the high readings and the frequency at which they occur. 
  

REED TEMPERATURE 

 
The F-2000R has been calibrated at 80°F on various samples and on different cuttings and 
mixtures. The higher the temperature of the sample, the higher the meter readings will be.  
Temperatures lower than 80°F cause lower meter readings.  The correction is approximately 
1% point for every 20°F/12°C difference.  Refer to chart below: 
 

Reed temperature 

Add to reading 

Subtract from reading 

20°F  / -7°C 

-- 

40°F  /  5°C 

-- 

60°F  / 15°C 

-- 

80°F  / 30°C 

100°F / 40°C 

-- 

120°F / 50°C 

-- 

140°F / 60°C 

-- 

 
Example: 
 
Meter reading  

: 22% 

Temperature   

: 40°F / 5°C 

Moisture Content 

: 24% (22 + 2) 

 

 
CURING 

 
Before proper curing has taken place, wide variations in moisture content should be 
expected in both reed stems and in the stacks. These variations will be exposed by meter 
readings taken on different parts of the bundle.  

The higher the moisture range, the 

wider are the variations.  The more curing has been allowed to take place, the 
greater uniformity in moisture distribution can be expected.   

 
The validity of the meter readings is closely related to the care spent in sampling the reed 
to be tested. A firm contact of the electrode with the reed is important. The number of tests 
made should be increased whenever the initial readings show considerable variations. 
 

DENSITY 

 
The calibration of the moisture testers applies to stacks of normal “average” density.  
Generally: 
 

 

High pressed stacks may yield readings 1-2% points higher.   

 

Loose pressed stacks tend to yield 1-2% point lower.   

 

Tests in stacked loose reed stems usually yield readings 2%-3% lower. 

 

 

USE OF PRESERVATIVES 

 
Reed preservative or stabilizers may also have an effect on meter readings.  Normally a 
reed bundle treated with preservative will read higher than a bundle of the same reed that 
had not been treated.  The readings typically increase by 2-4% points, and 24-48 hours 
after treatment, the readings between the stacks tends to equalize. 
 

Содержание F-2000R

Страница 1: ...F 2000R REED MOISTURE METER OPERATION MANUAL DELMHORST EUROPE TITANIUMLAAN 100 NL 5221 CK s HERTOGENBOSCH THE NETHERLANDS info delmhorst eu www MoistureMetersDelmhorst com 31 0 73 6395080...

Страница 2: ...ng A Reading 6 Testing Reed stems 6 Testing in Roofing sheets 6 Factors Affecting Your Reading 6 Range Of Moisture Content 7 Reed Temperature 7 Curing 7 Density 7 Use Of Preservatives 8 In general 8 C...

Страница 3: ...ibration Displays the average of up to 100 accumulated readings displays the highest stored reading erases the readings Set Point Decrease 3 Acts as an arrow button when pressed after the set point bu...

Страница 4: ...e the button to stop at your desired set point If the meter reads a MC higher than that of the set point a buzzer will sound TO CHECK THE ACCUMULATED READINGS This feature allows you to view the total...

Страница 5: ...1235 to the external connector on the top of the meter Insert the electrode into the reed bundle Press the read button 1 The meter displays the MC for two seconds NOTES The reed electrode is electrica...

Страница 6: ...the electrical meter readings the indicated moisture content should not be used as an absolute quantitative measurement Meter readings are very useful guidelines for safe use of reed Meter readings b...

Страница 7: ...en on different parts of the bundle The higher the moisture range the wider are the variations The more curing has been allowed to take place the greater uniformity in moisture distribution can be exp...

Страница 8: ...ations among readings are greater If there is a possibility of high moisture areas samples from these locations should be taken Areas of high moisture content will spoil resulting in loss It is extrem...

Страница 9: ...prepaid We are not responsible for damage in transit We do not accept COD shipments or cover any incoming freight or duty charges on returned merchandise Turnaround time on repairs is approximately t...

Страница 10: ...MHORST be liable for any incidental indirect special or consequential damages of any type whatsoever including but not limited to lost profits or downtime arising out of or related in any respect to t...

Страница 11: ...Directive Standard s to which Conformity is declared EN 50082 1 1992 EMC Generic immunity standard EN 50081 1 1992 EMC Generic emission standard EN 55011 1991 Limits and methods of measurement of radi...

Страница 12: ...12...

Отзывы: