4 Portions of the weld
run do not fuse to the
surface of the metal
or edge of the joint.
A
B
Small electrodes used on heavy
cold plate.
Welding current is too low.
A
B
Use larger electrodes and
pre-heat the plate.
Increase welding current.
C Wrong electrode angle.
C Adjust angle so the welding arc is
directed more into the base metal.
D Travel speed of electrode is
too high.
D Reduce travel speed of electrode.
E Scale or dirt on joint surface.
E Clean surface before welding.
Table 10-2 (continued): Stick Welding Problems
Lack of fusion caused by dirt,
electrode angle incorrect,
rate of travel too high
Lack of side fusion, scale
dirt, small electrode,
amperage too low
Lack of inter-run
fusion
Lack of root fusion
Art # A-04992
Figure 10-2: Example of Lack of Fusion
Содержание TRANSTIG 300 AC/DC
Страница 8: ......
Страница 20: ...TRANSTIG 300 AC DC SERVICE MANUAL 2 6 June 30 2008 THIS PAGE LEFT INTENTIONALLY BLANK...
Страница 34: ...TRANSTIG 300 AC DC SERVICE MANUAL 5 2 June 30 2008 NOTES...
Страница 56: ...TRANSTIG 300 AC DC SERVICE MANUAL 11 2 June 30 2008 NOTES...
Страница 78: ...THIS PAGE LEFT INTENTIONALLY BLANK TRANSTIG 300 AC DC SERVICE MANUAL 13 18 June 30 2008...
Страница 125: ...THIS PAGE LEFT INTENTIONALLY BLANK TRANSTIG 300 AC DC SERVICE MANUAL June 30 2008 A 7...