安德利
TIG-250GPLC
23
3
:把焊机转换到氩弧模式下,电流设置到
160
左右,把钨针和地线直接接触形成短路,按住
枪开关不放保持
2
到
3
秒钟左右,此时钨针产生高温可有效的把氧化层烧掉。此方法处理后钨
针应呈黑色,再次转换到冷焊模式下进行点焊即可。
3: Switch welding machine to argon arc mode, current is set at about 160, make tungsten
needle directly contact with welding spot to generate short circuit, press and hold onto gun
switch for 2 to 3 seconds, then high temperature generated by tungsten needle can burn
away oxidation layer effectively. Tungsten needle should present black color after being
treated by this method, and then switch to cold welding mode again to carry out spot welding.