1

:请按照安装示意图正确的连接好焊枪,控制线及地线。所有接头务必连接紧固以防接

触不良造成焊机连接端子损坏。

1:

Please connect welding gun, control line and ground wire correctly in accordance with

installation diagram. All connectors must be connected and fastened so as to prevent

damage of terminal block of welding machine due to poor contact.

2

:请确保氩气管与焊机连接紧固密封,以防漏气,影响焊点质量

2:

Please be sure that argon tube and welding machine are connected, fastened and

sealed so as to prevent air leakage and influencing quality of welding spot.

3

:将焊机后面的接地螺丝用大于

4

平方的导线可靠接地,防止静电及漏电发生。

3:

Use wire which is greater than 4mm

2

to earth grounding screw behind the wielding

machine so as to prevent occurrence of static electricity and electric leakage.

氩弧焊操作方法:

Operation method of argon arc welding:

1

:打开氩气瓶的阀门并调好流量计至所需的流量。

1:

Turn on valve of argon gas bottle and adjust flowmeter to required flow.

2

:按下焊枪开关,电磁阀工作,枪头开始有氩气流出。

2:

Press welding gun switch, solenoid valve starts working and argon gas starts to

outflow from gun head.

3

:将钨极与工件距离

2

3

个毫米,按下焊枪开关开始引弧,根据工件厚度设置好适当

的焊接电流即可。

3:

Adjust distance between tungsten electrode and workpiece to 2~3 millimeters, press

welding gun switch to start striking the arc, set up proper welding current according to

thickness of workpiece.

连续脉冲点焊操作方法:

Operation method of continuous pulse spot welding:

1

:在连续脉冲点焊模式下需要设置三个参数:焊接电流,点焊时间,点焊频率用户可根

据工件的厚度设置适当的电流与点焊时间,点焊频率。然后按住枪开关不放以一定的速
度拖动焊枪移动即可焊出鱼鳞状的焊道,要结束焊接,松开枪开关即可。注意:在焊接
薄板时钨针和板的距离应控制在

0.5

毫米以下为佳。

1:

Three parameters need to be set up in the mode of continuous pulse spot welding:

welding current, spot welding time and spot welding frequency. User may set up

proper current, spot welding time and spot welding frequency in accordance with

thickness of workpiece. Then press and hold onto gun switch, drag welding gun to

move at a certain speed, weld scaly welding bead, and just loosen gun switch to stop

welding. Notes: when welding thin plate, the best distance between tungsten needle

and plate shall be controlled smaller than 0.5 millimeter.

2

:点焊频率与拖动焊枪移动的速度有着密切的关系,点焊频率低焊枪移动的速度应慢,

过快的速度会导致焊点与焊点之间连接不上影响焊接质量。点焊频率高焊枪移动的速度
应加快,频率越高焊道鱼鳞状越密。

2:

Spot welding frequency and speed of dragging welding gun are closely related, if spot

welding frequency is low, speed of moving welding gun shall be slow, fast speed will

lead to failure in connection between welding spots and influence welding quality. If

spot welding frequency is high, speed of moving welding gun shall be accelerated,

the higher the frequency, the denser of scaly welding beads.

3

:在连续脉冲点焊模式下,用户应根据工件的实际情况对焊接的参数进行多次调式,试

焊,以达到工艺要求为准。

3:

In the mode of continuous pulse spot welding, user should repeatedly debug and test

Содержание TIG-250GPLC

Страница 1: ...1...

Страница 2: ...2 TIG 250GPLC TIG 250GPLC Intelligent Precision Multifunction Argon Arc Welding Machine User Manual Please read carefully before use...

Страница 3: ...1 1 2 2 3 3 4 4 5 6 1 Matters needing attention for safety operation 1 2 Product overview 2 3 Main technical parameters electrical principle block diagram 3 4 Panel control and operation 4 5 Installat...

Страница 4: ...rs Solemn Statement GB 15579 1 2013 ANDELI ANDELI GROUP CO LTD solemnly and sincerely declares that this product is manufactured in accordance with relevant Chinese and international standards and con...

Страница 5: ...sure not to carry out hot line work Electric shock might lead to serious injury and even death Install grounding device in accordance with application standard It is forbidden to contact with live par...

Страница 6: ...afety Be sure that fire extinguishing apparatus is available nearby and trained personnel can operate fire extinguisher skillfully Please don t weld sealed combustion vessel It is forbidden to use wel...

Страница 7: ...ual or still can t solve the problem in accordance with the User Manual you should contact with your supplier or service center of ANDELI Company immediately to seek professional help 2 2 Product over...

Страница 8: ...continuous pull welding of thin plate Single spot cold welding technology can perfectly overcome difficulty in spot welding of thin plate Beautiful modeling and structure design Streamline modeling de...

Страница 9: ...oltage 56 V Pulse continuous spot welding frequency 1 30HZ Regulating range of pulse time 1 200 Regulating range of cold welding current 5 200A Preflow time 0 1S Gas delay time 0 5 5S Rated load susta...

Страница 10: ...ANDELI TIG 250GPLC 10 Electrical principle block diagram Power switch Driver module Power supply Feedback Control circuit...

Страница 11: ...welding Single spot cold welding Time display Time adjustment Welding gun Front panel Welding gun switch Current display Pulse spot welding frequency Current regulation pulse frequency Press Selectio...

Страница 12: ...justment Argon arc welding mode Spot welding time display Spot welding time adjustment Spot welding frequency display Spot welding frequency adjustment Continuous pulse spot welding mode Notes welding...

Страница 13: ...ANDELI TIG 250GPLC 13 Welding current adjustment Single spot cold welding mode...

Страница 14: ...r which corresponding voltage class is greater than 34A or electric wire which is greater than 4mm2 in accordance with input current and voltage of welding machine Be sure not to connect with wrong vo...

Страница 15: ...ANDELI TIG 250GPLC 15 Installation diagram Distribution box Argon gas bottle Ground connection Argon welding gun Workpiece...

Страница 16: ...up proper welding current according to thickness of workpiece Operation method of continuous pulse spot welding 1 0 5 1 Three parameters need to be set up in the mode of continuous pulse spot welding...

Страница 17: ...shares welding current in this mode please convert to argon arc mode in case of setting welding current adjust and then switch back to this mode Please refer to panel operation and control descriptio...

Страница 18: ...e 70 90 30 50 Tungsten needle angle 30 50 Tungsten needle installation schematic diagram 5 8 Tungsten electrode stretching out of porcelain mouth shall be subject to 5 8 millimeters the best Slab spli...

Страница 19: ...tion of tungsten needle and influence welding quality 3 0 3 0 4 3 Be sure to fixate two planes to be welded by several welding spots before carrying out spot welding for workpiece and align tungsten n...

Страница 20: ...another welding spot till completion of spot welding Notes beginner usually finds adhesion of tungsten needle and workpiece which is normal and be able to avoid or reduce such phenomenon by controllin...

Страница 21: ...rent 160 170 Spot welding time 20 40 Color coated plate splicing spot welding 0 5 130 150 6 8 Thickness 0 5 millimeter 0 8 Welding current 130 150 150 160 Welding time 6 8 8 12 Thickness 0 8 millimete...

Страница 22: ...g user should pay close attention and listen to the sound when carrying out spot welding sound is very pure when carrying out spot welding normally and there is no noise In case of any squeak tungsten...

Страница 23: ...act with welding spot to generate short circuit press and hold onto gun switch for 2 to 3 seconds then high temperature generated by tungsten needle can burn away oxidation layer effectively Tungsten...