Gel Coat

Discolored areas are very shallow in 

depth, literally right on the surface. The 

discoloration may be removed by gently 

wet-sanding the affected areas only by 

using 600 grit, wet or dry specially treated 

waterproof sandpaper. It’s important to 

always sand in one direction, this includes 

the curves too. Use plenty of water to cool 

and clean the sandpaper and cut back on 

dust. After  you are finished sanding, dry 

the areas and verify all the discoloration 

has been removed. If not, repeat the 

process. 

After all the discoloration has been 

removed, the area will need to be buffed. 

Using an electrical or pneumatic buffer, 

buff at low speed (1750 rpm – 2250 rpm), 

this will restore the luster to the sanded 

surface. Using a generous amount of 

rubbing compound, apply it in a circular 

motion with a soft wool pad. When buffing 

has been completed, wash off the rubbing 

compound with clean water, and dry the 

surface.

To restore the gloss to the affected area, 

use a high-grade marine or automotive 

wax.

Repairs

During the life of your boat, some damage 

to the gel coat surface is unavoidable. 

We recommend repairs done by trained, 

experienced professionals at your local 

marine dealer.

Scratches

If the scratch is in the gel coat surface, 

not penetrating the fiberglass, use an 

automotive polishing compound and rub it 

out. Apply the compound by hand using a 

damp rag or by using a power buffer. The 

scratch may not entirely disappear, but it 

should be noticeably better.

Gouges and Chips

Our recommended patching procedure is 

to first clean the area needing repair with 

an acetone solvent to remove all traces 

of wax and oil. Next, thoroughly mix one 

tablespoon of “Patch Paste” with two or 

three drops of catalyst on a scrap piece of 

cardboard.

Apply the mixture to the pit, chip or gouge 

with a single-edge razor blade, matching 

the surface and contour of the area being 

repaired. Apply slightly more mixture to 

avoid having to fill the damaged section 

a second time. Allow the patch to harden 

thoroughly for a minimum of two to three 

hours.

Using a fine grit “wet or dry” sandpaper on 

a sanding block, wet-sand the patch until 

it is level with the surrounding surface. 

Finish with a marine or automotive rubbing 

compound using the same approach as 

used for the scratches.

Refinishing

For a severely scratched or weathered 

fiberglass boat that is no longer restorable 

by using the previous methods, it may then 

be necessary to refinish it with two-pack-

age or two-part aliphatic urethane enamel. 

This can be done very effectively, but it is 

recommended refinishing should only be 

done by experienced professionals.

Summary of Contents for 1900 BB

Page 1: ...10 15 2014 Sailfish 290CC Owner s Manual sailfishboats com 1 01 27 2015 Sailfish 1900 BB Owner s Manual sailfishboats com 1 Sailfish 1900 BB Title Demand The Difference Sailfish 1900 BB Owner s Manual...

Page 2: ...m 9 UFLEX STEERING 10 Ignition Switches Engine Shut Off Cord Lanyard 11 Fuel Water Separator Yamaha 11 Plug and Play Wiring 12 Console Area 13 Bilge Pump 14 Raw Water Washdown System 15 Livewell Opera...

Page 3: ...ll Boat Carbon Fiber Kevlar Reinforced Deck Hull Closed Cell Foam Flotation Boarding Ladder Swim Platform SailTech Composite Full Length Transom SailTech Foam Filled Fiberglass Stringer System Stainle...

Page 4: ...n 2100 BB 88 in 66 in 37 in 10 5 in 99 5 in 220 in 240 in 24 in 220 CC WAC 87 in 59 in 31 in 14 5 in 102 5 in 216 5 in 243 in 32 in 240 CC WAC 92 in 59 in 31 in 15 in 107 in 241 in 272 in 30 in 220 CC...

Page 5: ...ption 1 Fishbox or Release Well 2 72 Quart Cooler Seat 3 Boarding Ladder 4 Battery Access and Storage Compartment 5 Console Helm Area Key Description 6 Front Helm Seat with Livewell 7 Insulated Fish B...

Page 6: ...01 27 2015 Sailfish 1900 BB Owner s Manual sailfishboats com 5 Bay Boat Wiring Harness...

Page 7: ...allation Perko Switch Perko Battery Switch on 1900BB 2100BB 208CC 220CC 220WAC Connect all ground wires to the negative post on battery 1 Perko battery switch has a 1 2 and ALL position to switch to W...

Page 8: ...ner s Manual sailfishboats com 7 Fuel System Layout q w e e e Key Description 1 Primer Bulb Yamaha only 2 Fuel Filter Access Yamaha Only 3 Fuel Tank Location 4 Inspection Plate 5 Fuel Fill 6 Fuel Pick...

Page 9: ...rolling motor routing fwd lockers drain fuel vent fuel fill rigging pipe livewell drain opt livewell livewell deck drain deck drain washdown fuel feed option release well fuel filter option aft releas...

Page 10: ...tandard with a full stainless steel shaft cylinders are built with carbon steel pistons coupled with extra large end caps to prevent leakage All of their connection materials are 304 stainless steel t...

Page 11: ...helm controls the lanyard will pull out causing the en gine to shut down Make sure the lanyard is not attached to a part of your clothing that could be easily torn free caus ing the switch not to pull...

Page 12: ...ese filters can be accessed in the bilge access door located at the aft of the boat For more information on these filters please review your Yamaha Owner s Manual Plug and Play Wiring Deutsch Connecto...

Page 13: ...s Manual sailfishboats com 12 Console Area Key Description 1 Guage and Switch Panel 2 Binnacle 3 Optional Trim Tabs 4 Helm with Steering Wheel 5 Ignition Switch Panel 6 Large Panels for easy access t...

Page 14: ...h causing the pump to turn on The pump will continue to run until enough water is removed for the float to drop back down disengaging the pump The pump also has a manual switch function on the main sw...

Page 15: ...nd pressure is created the pump will shut down until more pressure is needed The raw water wash down pump can be accessed through the aft starboard hatch To operate make sure the seacock is in the ope...

Page 16: ...urn on the livewell switch Adjust the black aerator in each livewell to the desired flow shown in CLOSED picture You can operate both at the same time or just one by adjusting the flow In order to fil...

Page 17: ...ainless steel must be kept clean and free of all these contaminants NOTE LENCO RECOMMENDS AN ACID AND WATER SOLUTION TO CLEAN THE TRIM TAB BLADES MARYKATE S ON OFF PRODUCT IS A GOOD CHOICE RINSE THOR...

Page 18: ...r cleaners may void your warranty damage your vinyl Do s Don ts Do s Vinyl Finish Vinyl Cleaner Dish Soap Dawn Ivory Fantastik 303 Aerospace Protectant Don ts Formula 409 Murphy s Oil Soap Simple Gree...

Page 19: ...to protect it as much as possible from pitting When the anodized coating is broken and raw aluminum is exposed corrosion will take place Damage from other abrasive impacts can break the anodized coati...

Page 20: ...ctive they are not one time solutions Metal protec tors must be reapplied on a regular basis How often a protector should be used varies according to the protector you choose the types of exposure you...

Page 21: ...nd 8 Nickel while 316 Contains 16 Chromium and 10 Nickel and 2 Molybdenum The Molybdenum is added to help resist corrosion to chlorides like sea water and de icing salts Can Stainless Steel rust Not i...

Page 22: ...ield first with lukewarm water to avoid scratching the surface WINDOW CHANNELS Clean window channels with mild deter gent only Channels can be sprayed with silicon aerosol while sliding the glass back...

Page 23: ...n application of rubbing compound and a thorough waxing Cleaning We recommend general washing to avoid soil build up and staining The soil to your gel coat is the result of regular use and environment...

Page 24: ...e dealer Scratches If the scratch is in the gel coat surface not penetrating the fiberglass use an automotive polishing compound and rub it out Apply the compound by hand using a damp rag or by using...

Reviews: