Hull damage falls into three categories:
•
SERIOUS – large hole, split, crack, or worse. Don’t be too distressed!
Get the remnants back to RS Sailing or send us a picture for
assessment.
•
MEDIUM – small hole or split. If this occurs during an event, sailing can
often be continued as long as leaking can be prevented by drying the
area and applying strong adhesive tape. CAUTION – if the damage is
close to a heavily loaded point, then the surrounding area should be
closely examined to ensure that it will accept the loads. Get the
damage professionally repaired as soon as possible.
•
SMALL – dents, scratching. This type of damage is not boat
threatening.
Comptec PE3 cannot be repaired in the same way as fibre glass. Some
scratching can be removed by RS Sailing staff, but dents cannot. Therefore
we suggest you treat your boat with as much care as you would if it were fibre
glass. More serious repairs can be carried out by RS Sailing staff; however,
the repair will never be invisible, due to the nature of the material.
The joy of owning an RS Cat 16 is that it is very hard wearing, and any dents
and scratches it receives will not affect the structural integrity of the hull.
39
Summary of Contents for RS Cat 16
Page 1: ...Owner s Manual v2...
Page 9: ...Assembly Guide 4 1 Hulls PLEASE FOLLOW ASSEMBLY GUIDE IN THE CORRECT ORDER 7...
Page 20: ...Assembly Guide 4 2 Mast PLEASE FOLLOW ASSEMBLY GUIDE IN THE CORRECT ORDER 18...
Page 24: ...10 S AND XL ONLY Add furler line 4 2 ASSEMBLY MAST 22...
Page 25: ...Assembly Guide 4 3 Sails PLEASE FOLLOW ASSEMBLY GUIDE IN THE CORRECT ORDER 23...
Page 28: ...Assembly Guide 4 4 Spinnaker PLEASE FOLLOW ASSEMBLY GUIDE IN THE CORRECT ORDER XL only 26...
Page 31: ...8 9 TACK H EAD Add spinnaker sheet Tidy slack into pocket 4 4 ASSEMBLY SPINNAKER 29...
Page 32: ...Assembly Guide 4 5 Foils PLEASE FOLLOW ASSEMBLY GUIDE IN THE CORRECT ORDER 30...
Page 33: ...1 2 4 5 ASSEMBLY FOILS 31...
Page 57: ......