5 Handling the Lead-free Solder
5.1. About lead free solder (PbF)
Distinction of PbF P.C.B.:
P.C.B.s (manufactured) using lead free solder will have a PbF stamp on the P.C.B.
Caution:
·
Pb free solder has a higher melting point than standard solder; Typically the melting point is 50 - 70°F (30 - 40°C) higher. Please
use a high temperature soldering iron. In case of soldering iron with temperature control, please set it to 700 ± 20°F (370 ±
10°C).
·
Pb free solder will tend to splash when heated too high (about 1100°F/600°C).
·
When soldering or unsoldering, please completely remove all of the solder on the pins or solder area, and be sure to heat the
soldering points with the Pb free solder until it melts enough.
8
SA-AK340GCP
Summary of Contents for SA-AK340GCP
Page 13: ...8 Operation Procedures 13 SA AK340GCP ...
Page 14: ...14 SA AK340GCP ...
Page 23: ...10 3 Main Parts Location 23 SA AK340GCP ...
Page 40: ...12 2 Checking and Repairing of Transformer P C B 40 SA AK340GCP ...
Page 41: ...12 3 Checking and Repairing of Panel Deck Deck Mechanism P C B 41 SA AK340GCP ...
Page 42: ...12 4 Checking and Repairing of Power P C B 42 SA AK340GCP ...
Page 47: ...47 SA AK340GCP ...
Page 48: ...14 2 Power P C B and Transformer P C B 48 SA AK340GCP ...
Page 49: ...14 3 Waveform Chart 49 SA AK340GCP ...
Page 50: ...50 SA AK340GCP ...
Page 52: ...52 SA AK340GCP ...
Page 58: ...58 SA AK340GCP ...
Page 60: ...SA AK340GCP 60 ...
Page 62: ...SA AK340GCP 62 ...
Page 68: ...SA AK340GCP 68 ...
Page 70: ...SA AK340GCP 70 ...
Page 74: ...SA AK340GCP 74 ...
Page 82: ...SA AK340GCP 82 ...
Page 87: ...21 Exploded Views 21 1 Cabinet Parts Location SA AK340GCP 87 ...
Page 88: ...SA AK340GCP 88 ...
Page 89: ...21 2 Deck Mechanism Parts Location RAA4502 S SA AK340GCP 89 ...
Page 90: ...21 3 Packaging SA AK340GCP 90 ...