English - 15 -
7.3. Compounds and their application
In general the compound SC 5 is used in the
Eco-mini „wet“
.
The compound SC 5 keeps the work-pieces clean and corro-
sion-free while grinding. Also, the sharpness of the chips is re-
tained, by using this compound.
SC 5 should be mixed with water as per the following instruc-
tions:
Add 0.5 liters of the compound SC 5 to 10 liters of water.
7.4. Processing examples
7.4.1. How to process jewelry straight from the casting
When you want to process jewelry straight from the casting, the
grinding should be done in two steps:
·
Fill the work-container with approximately 1,5 liters blue
plastic chips PO 10 (pyramids) .
·
Select the processing time by turning the timer clockwise.
The machine will now start.
·
Processing time to grind gold and silver: 2-3 hours
·
Processing time to grind platinum, titanium and
stainless steel: 6-12 hours
·
The machine will switch off automatically after the time set
has expired.
·
Unload the work-container completely and separate the blue
chips from the work-pieces.
·
Fill the work-container with the white cones KX 10.