OM-230 693 Page 43
8-14. Troubleshooting − Waviness Of Bead
Waviness Of Bead − weld metal that is not parallel and does not cover
joint formed by base metal.
S-0641
Possible Causes
Corrective Actions
Welding wire extends too far out of nozzle.
Be sure welding wire extends not more than 1/2 in (13 mm) beyond nozzle.
Unsteady hand.
Support hand on solid surface or use two hands.
8-15. Troubleshooting − Distortion
Distortion − contraction of weld metal during welding that forces
base metal to move.
Base metal moves
in the direction of
the weld bead.
S-0642
Possible Causes
Corrective Actions
Excessive heat input.
Use restraint (clamp) to hold base metal in position.
Make tack welds along joint before starting welding operation.
Select lower voltage range and/or reduce wire feed speed.
Increase travel speed.
Weld in small segments and allow cooling between welds.
Summary of Contents for Millermatic 252
Page 14: ...OM 230 693 Page 10...
Page 25: ...A complete Parts List is available at www MillerWelds com OM 230 693 Page 21 Notes...
Page 27: ...A complete Parts List is available at www MillerWelds com OM 230 693 Page 23 226 650 B...
Page 37: ...OM 230 693 Page 33 Notes...
Page 38: ...OM 230 693 Page 34 SECTION 7 ELECTRICAL DIAGRAM Figure 7 1 Circuit Diagram...
Page 39: ...OM 230 693 Page 35 229 485 A...