background image

2

KODAK PRECISION LINE Contact Film UCA7 

 TI-2037

RECIPROCITY

With recommended processing, the reciprocity speed change 
is negligible (1/3-photographic stop or less) within exposure 
range of 1/1000 second to 100 seconds; there is no change in 
contrast.

PROCESSING

Notice: 

Observe precautionary information on product labels and on 

the Material Safety Data Sheets.

Use KODAK ACCUMAX Rapid Access Developer and 

Replenisher (diluted 1:2) and KODAK PROFESSIONAL 
Rapid Fixer and Replenisher (diluted 1:3). Do not use any 
type of hardener in the fixer.

Size

CAT No.

KODAK ACCUMAX Rapid 
Access Developer and 
Replenisher

5 L concentrate

887 5569

KODAK PROFESSIONAL 
Rapid Fixer and 
Replenisher

5 L concentrate

174 9839

Recommended Starting Points:

Fixer:

 Use a fixer temperature of 32 - 35

°

C (90 - 95

°

F).

Replenishment Rates:

Developer

Temperature

Time

(Seconds)

ACCUMAX Developer

38

°

C (100

°

F)

30 seconds

35

°

C (95

°

F)

45 seconds

32

°

C (90

°

F)

60 seconds

RA 2000 Developer Repro Developer (Liquid)

35

°

C (95

°

F)

30 seconds

32

°

C (90

°

F)

45 seconds

Developer

Fixer

350 mL / sq m

540 mL / sq m)

Summary of Contents for TI-2037

Page 1: ...in up to 40 footcandles 430 lux of roomlight illumination substantially free of ultraviolet UV energy Such illumination is supplied by yellow fluorescent lamps warm white preferred and white fluorescent lamps covered by UV absorbing or modified by UV absorbing plastic diffusers Other roomlight sources contain varying amounts of UV energy and their roomlight tolerances for this film should be teste...

Page 2: ...luted 1 2 and KODAK PROFESSIONAL Rapid Fixer and Replenisher diluted 1 3 Do not use any type of hardener in the fixer Size CAT No KODAK ACCUMAX Rapid Access Developer and Replenisher 5 L concentrate 887 5569 KODAK PROFESSIONAL Rapid Fixer and Replenisher 5 L concentrate 174 9839 Recommended Starting Points Fixer Use a fixer temperature of 32 35 C 90 95 F Replenishment Rates Developer Temperature T...

Page 3: ...y vary slightly in different directions within a sheet the differences that may exist however are not always equal between the length and width directions Differences in size change between length and width directions should be within 10 percent of each other CURVES Characteristic Curve 95F 22 sec LOG EXPOSURE lux seconds 0 0 0 0 2 0 DENSITY 1 0 2 0 3 0 7 0 3 0 4 0 Densitometry Exposure Process RA...

Page 4: ...roduct characteristics at any time Aerial and Industrial Markets Business EASTMAN KODAK COMPANY ROCHESTER NY 14650 MORE INFORMATION For the latest version of technical support publications for Kodak products visit Kodak on line at http www kodak com go PCBproducts If you have questions about Kodak products call Kodak In the U S A 1 800 242 2424 Ext 19 Monday Friday 9 a m 7 p m Eastern time In Cana...

Reviews: