10 Preparing the Welding Head
Stud welding with drawn arc under shielding gas
Make sure that you have inserted the pressure spring (order no. 80-10-
400) for the gap welding process and that the toggle switch for solenoid is
set to the
ON position
.
If not observed, you will obtain poor welding results.
Stud welding units
ARC 800 *) / ARC 1550 *)
Material
of welding elements
Diameter of welding elements
Welding parameters
Metric
KAH 412
PT, UT
IT
Lift
in mm
Spring force
in mm
Material of workpiece: Mild steel (suitable for welding)
4.8 (suitable for welding)
M3, 3 mm
--
1.0
5
4.8 (suitable for welding)
M4, 4 mm
--
1.0
5
4.8 (suitable for welding)
M5, 5 mm
5 mm, M3
1.0
5
4.8 (suitable for welding)
M6, 6 mm
6 mm, M4
1.0
5
4.8 (suitable for welding)
M8, 7.1 mm
7.1 mm, M5
1.5
5
Material of workpiece: Galvanised steel (suitable for welding)
4.8 (suitable for welding)
M3, 3 mm
--
1.2
5
4.8 (suitable for welding)
M4, 4 mm
--
1.2
5
4.8 (suitable for welding)
M5, 5 mm
5 mm, M3
1.4
5
4.8 (suitable for welding)
M6, 6 mm
6 mm, M4
1.4
5
4.8 (suitable for welding)
M8, 7.1 mm
7.1 mm, M5
2.0
5
Material of workpiece: Alloyed steel (suitable for welding)
A2-50
M3, 3 mm
--
1.0
5
A2-50
M4, 4 mm
--
1.0
5
A2-50
M5, 5 mm
5 mm, M3
1.0
5
A2-50
M6, 6 mm
6 mm, M4
1.0
5
A2-50
M8, 7.1 mm
7.1 mm, M5
1.5
5
*)
can only be used with the automatic version