DUTY CYCLE & WELDING ENVIRONMENT DURING USE
• The welding unit describes an output characteristic of "constant current" type. The duty cycles following the stan
-
dard EN60974-1 (at 40°C on a 10mn cycle) are indicated in the table below :
NOVOMIG 110
X%-max
6% - 85A
12%
65A
During intensive use (> duty cycle) the thermal protection can activate, if this event the arc switches off and the ther
-
mal protection indicator switches on. The welding machine has a constant voltage output.
Note: The machines’ duty cycle has been tested at room temperature (40°C) and has been determined by simulation;
RISK OF INJURY DUE TO MOVING PARTS
The wire feeders contain moving parts that may catch hand, hair, clothes or tools which can lead to injuries!
Take extra care.
• Do not lay a hand to swivel or moving components or parts to the drive!
• Ensure that the housing covers or protective covers remain closed during operation!
TROUBLESHOOTING
SYMPTOMS
POSSIBLE CAUSES
REMEDIES
The welding wire speed is not
constant.
Debris is blocking up the opening.
Clean out the contact tip or change it
and replace the anti-adherence product.
Ref.041806
The wire skids in the rollers
Check the roller pressure or replace it.
- Wire diameter incompatible with roller
- Covering Wire guide in the torch incompatible
The wire-feeder motor doesn’t operate.
Reel or roller brake too tight
Adjust the brake and rollers.
Electrical supply problem.
Check the power switch is in the "On" position.
Bad wire feeding.
Covering wire guide dirty or damaged
Clean or replace
Reel brake too tight
Release the brake
No welding current
Bad connection to the main supply
Check the mains connection and ensure the
supply is 230V (1PH) power socket.
Bad earth connection.
Check the earth cable (connection and clamp
condition).
The wire jams (after the rollers).
Guide wire sheath crushed.
Check the sheath and torch body.
Wire jammed in the torch
Clean or replace.
No capillary tube.
Check the presence of capillary tube.
Wire speed too fast
Reduce the wire speed.
The welding bead is porous.
Nozzle dirty
Clean or replace nozzle.
Poor quality wire.
Use suitable wire for no gas welding.
Work piece in bad condition. (rust, etc…)
Clean the metal before welding.
The arc produces a lot of sparks
Arc voltage too low or too high.
See welding settings.
Bad earth connection.
Adjust the earth cable for a better connection.
Summary of Contents for NOVOMIG 110
Page 30: ...30 NOVOMIG 110 RU 10 40 C 14 104 F 20 55 C 4 131 F 50 40 C 104 F 90 20 C 68 F 1000 3280 10...
Page 31: ...31 NOVOMIG 110 RU 11 2 CLASSIFICATION CEM DU MAT RIEL A CEI 61000 3 12 CEM EMF...
Page 32: ...32 NOVOMIG 110 RU EMF b c d e f g h 10 CISPR 11 2009 a...
Page 33: ...33 NOVOMIG 110 RU b c d e f 10 IP21 12 5...
Page 37: ...37 NOVOMIG 110 RU NO GAS...
Page 53: ...53 NOVOMIG 110 FIG I FIG II 3 5 7 10 9 2 1 6 8 4...