background image

W

eld Speed  Too Fast

TO CORRECT

:

weld 

slower

W

eld Speed  Too Slow

TO CORRECT

:

weld  faster

Arc Length 

 

Too Short

TO CORRECT

:

Good 

 

W

eld

Arc Length 

 

Too Long

TO CORRECT

:

50 AMP 

ARC

 WELDER

O

VERL

O

AD

MIN

CURRENT

MAX

OFF

ON

PO

WER

I

O

Current 

 

Too High

TO CORRECT

:

50 AMP 

ARC

 WELDER

O

VERL

O

AD

MIN

CURRENT

MAX

OFF

ON

PO

WER

I

O

Current 

 

Too Low

TO CORRECT

:

CLEAN WELDS FIRST!

   

Stick welds will have a coat of slag over them until cleaned.

68888

 

WELD EXAMPLE PICTURES

All manuals and user guides at all-guides.com

Summary of Contents for 68888

Page 1: ...t current setting as needed HOLD ELECTRODE CLEAR 5 Hold electrode clear of workpiece then plug in welder and turn it on 20 amp minimum circuit 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O 3 Attach ground clamp to workpiece 2 Clamp bare end of electrode in holder All manuals and user guides at all guides com a l l g u i d e ...

Page 2: ... Long TO CORRECT 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O Current Too High TO CORRECT 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O Current Too Low TO CORRECT CLEAN WELDS FIRST Stick welds will have a coat of slag over them until cleaned 68888 WELD EXAMPLE PICTURES All manuals and user guides at all guides com ...

Page 3: ...o MANTENGA EL ELECTRODO ALEJADO 5 Mantenga el electrodo alejado de la pieza de trabajo luego enchufe la soldadora y enciéndala Circuito mínimo de 20 amp 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O 3 Coloque la abrazadera de conexión a tierra en la pieza de trabajo 2 Fije el extremo descubierto del electrodo en el soporte A...

Page 4: ...uy larga PARA CORREGIR 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O Corriente muy alta PARA CORREGIR 50 AMP ARC WELDER OVERLOAD MIN CURRENT MAX OFF ON POWER I O Corriente muy baja PARA CORREGIR PRIMERO LIMPIE LAS SOLDADURAS Las soldaduras de barra tienen una capa de escoria arriba que se retira al limpiarlas 68888 IMÁGENES DE EJEMPLO DE SOLDADURAS All manuals and user guides at all ...

Reviews: