9
260º
: Use ABS or materials with a similar melting temperature
range for materials over 260º. Start extruding until no trace
of the previously used material remains. Once this point is
reached, progressively lower the temperature to 250º.
260º
: Use polypropylene for materials less than 260º. Start
extruding until no trace of the previously used material remains.
Once at this point, progressively lower the temperature to 210º.
Print Bed Setting
• During printing, fine-tune using Z Babysteping until proper adhesion is achieved
Advanced
• If you want to modify the number of points to be polled, you can make the changes from System / Config.g
• Go to ; Probe Z and change the P parameter of the following command
M557 X15:215 Y15:195P3:3
• You can also download or edit your heihtmap.csv file to correct any point or to save different height maps created
Load Compression Map
• If you have restarted the printer, you must load the Height Map again, to do this, execute Load Height Compensation Map
saved in the SD card (G29 S1)