After feeding welding rod the rotation rates of motor will become heavier, if it
becomes very difficult, please stop immediately, may be the screw heating time is too
short or the temperature is not high enough. Or the temperature is so high that lead to
the cut solder particle has been melt and clinging to the cutting blade to cause the
plugging before it falls into the extrusion gun body. In this case, it is necessary to
remove the Y type extrusion gun body and clean the scrap on the cutting blade to
ensure that the equipment is not damaged normally.

6. Faster welding speed need to higher heating temp. At general condition, the hot air

temperature is between 260

to 450

. Choose suitable hot air temperature is

important during welding.

7. Adjusting the temperature and speed to make sure the welding rod is melting and
extruding perfectly when actual operation.

8. The operator needs to press the hand extruder on welding seam during operating,
to make sure the melting material can bond well on seam.

9. Flat welding shoe and 90-degree welding shoe suitable for different welding ways.
Pls rotate and pull out of the welding shoe or preferably with a little heat and remove
when you need to replace it, do not pull or knock directly.

10.

Finishing stage:

Extrude all welding rods which inside the cylinder (when the

motor voice getting lighter that means extrude completely), and clean out the welding
materials that on the air outlet. Otherwise it may cause blocked when you use next
time.

11.

Shutdown stage:

Adjust the hot air gun to cold wind and cooling the heating

element at least 5 minutes before shutdown.
12. It needs to clear out all previous welding rods before next time to starting the
hand extruder up.
13. The service life of carbon brush around 1600 hours, pls note that and replace it
timely.

Содержание PW601

Страница 1: ...Shanghai Pengwang Machinery Co Ltd Address Building 8 No 1098 Chuansha road Pudong New Area Shanghai Sales phone 86 15801732387 PW601 Metabo Extruder Manual...

Страница 2: ...ngs welding repairing stitching sealing etc Especially for plastic pipe with large diameter 3 Thick plastic film geomembrane splicing repairing and so on Notice 1 CAUTION DANGER Please confirm that th...

Страница 3: ...Rod DIA 3 5 4 5mm Welding Speed 1 8 3 6kg h Welding Material HDPE PP PVC PVDF Main Components and Name 1 Heating Element 6 Handle 11 Dust Shield 2 Y Style Extrusion Gun Body 7 Power Cord Plug 12 Moto...

Страница 4: ...reheating time is too long the heat of the outlet will fall back which will cause the motor overheated and stopped The welding rod will be melted before it enters the extrusion chamber and the blade c...

Страница 5: ...lding rod is melting and extruding perfectly when actual operation 8 The operator needs to press the hand extruder on welding seam during operating to make sure the melting material can bond well on s...

Страница 6: ...h of the welding gun Do not operate for a long time to prevent the motor from overheating Caution Do not increase the motor speed unilaterally without increasing the heating temperature Otherwise the...

Страница 7: ...ating pipes that are not produced by our company 4 The normal wear and tear of the machine is not warranted 5 The damage caused by non resistance such as lightning flood fire accident and other non ma...

Страница 8: ...the screw or blade Welding rod pellet stuck the blade and feed screw Take apart the cylinder remove the pellet Drive motor was stop Carbon brush was wear after over the service life Replace the carbon...