6-19
Chapter 6
W
elding Condition
S
ETTING
W
ELDING
C
ONDITIONS
W
ELDING
C
ONDITION
C
HAPTER
6
T I P S
• Even in the Crater-fill off mode, using the internal function (F45) enables to carry out the
welding process in the initial condition before the main welding, and the welding process in
the Crater condition after the main welding. (
sequence (effective/initial standard time setting/crater standard time setting))
6.6.3.1
Crater "OFF"
Select "CRATER OFF" by the CRATER-FILL key.
•
In synchronous to the ON/OFF operation of the torch switch, the welding starts/stops.
10
no pulse
DC PULSE/
DC WAVE PULSE
HIGH
-
Al/Mg
11
no pulse
DC PULSE/
DC WAVE PULSE
HIGH
-
Brazing Cu Si
12
no pulse
DC PULSE/
DC WAVE PULSE
HIGH
-
Brazing Cu Al
Pattern No.
Crater setting
WELDING METHOD
TRAVEL SPEED
GAS
WIRE MATERIALS
Torch switch
Gas flow
Output voltage
Wire feeding speed
Welding current
Main welding
Anti-stick time
ON
OFF
Pre-flow
Post-flow
No-load voltage
Slow-down speed
Welding current
ON
OFF
Содержание OTC Welbee P500L
Страница 2: ......
Страница 8: ...TABLE OF CONTENTS vi MEMO...
Страница 142: ...TROUBLESHOOTING TROUBLESHOOTING CHAPTER 9 9 6...
Страница 158: ...MATERIALS FOR SETTING WELDING CONDITIONS REFERENCE MATERIALS CHAPTER 10 10 16...