Emissivity Table
Material
Temp C/ F
° °
Emissivity
Gold(
pure highly polished
)
227/440
0.02
Aluminum foil
27/81
0.04
Aluminum disc
27/81
0.18
Aluminum household(
flat
)
23/73
0.01
577/1070
0.06
Aluminum(
rough plate
)
26/78
0.06
Aluminum(
oxidized @599 C
)
°
199/390
0.11
599/1110
0.19
Aluminum surfaced roofing
38/100
0.22
Tin(
bright tinned iron sheet
)
25/77
0.04
Nickel wire
187/368
0.1
Lead(
pure 99.95-unoxidized
)
127/260
0.06
Copper
199/390
0.18
599/1110
0.19
Steel
199/390
0.52
599/1110
0.57
Zinc galvanized sheet iron(
bright
) 28/82
0.23
Brass(
highly polished
):
247/476
0.03
Brass(
hard rolled-polished w/lines
): 21/70
0.04
Iron galvanized(
bright
)
-
0.13
Iron plate(
completely
)
20/68
0.69
Rolled sheet steel
21/71
0.66
Oxidized iron
100/212
0.74
Wrought iron
21/70
0.94
Molten iron
1299-1399/3270-2550
0.29
Copper(
polished
)
21-117/70-242 0.02
Copper(
scraped shiny not mirrored
) 22/72
0.07
Copper(
Plate heavily oxidized
)
25/77
0.78
Enamel(
white fused on iron
)
19/66
0.9
Formica
27/81
0.94
Frozen soil
-
0.93
Brick(
red-rough
)
21/70
0.93
Brick(
silica-unglazed rough
)
1000/1832
0.8
Carbon(
T-carbon 0.9% ash
)
127/260
0.81
Concrete
-
0.94
Glass(
smooth
)
22/72
0.94
Granite(
polished
)
21/70
0.85
Ice
0/32
0.97
Marble(
light gray polished
)
22/72
0.93
Asbestos board
23/74
0.96
Asbestos paper
38/100
0.93
371/700
0.95
Asphalt(
paving
)
4/39
0.97
Aluminum (
polisned prate 98.3%
)