80
GB/MT
V
W
However, it is no longer expedient for
thicker materials. In this case, it is better
to prepare a joint as shown below, in
which the edge of the plate is angled
(Fig. X).
X
Fillet weld connections
A fillet weld is created if the workpieces
are perpendicular to each other. The
weld should be shaped like a triangle
with sides of equal length and a slight
fillet. (Fig. Y, Z).
Welds on an inner edge
The preparation for this weld joint
is very simply and is carried out for
thicknesses of 5 mm. The dimension
“d” needs to be reduced to a minimum
and should always be less than 2 mm
(Fig. Y).
Y
However, it is no longer expedient for
thicker materials. In this case, it is better
to prepare a joint as shown in Figure X,
in which the edge of the plate is angled.
Z
Overlap welds
The most common preparation is that
with the straight weld edges. The weld
can be released using a standard angle
weld seam. Both workpieces must
be brought as close to each other as
possible, as shown in Fig. AB.
AB
Using the device
Summary of Contents for PMSG 200 A1
Page 3: ...1 2 10 36 3 7 A B C D 11 13 12 14 15 17 21 22 23 24 18 19 20 16 9 35 37 32 4 6 8 34 5 33 38...
Page 4: ......
Page 116: ...115 DE AT CH...
Page 117: ...116 DE AT CH...