28
www.longer3d.com
9. Printing Cases
Printing parameters:
Exposure time-6000ms, bottom time-80000ms
Layer thickness-50μm, Bottom height-0.3mm
Lift Distance1-2mm, Lift Speed1-48mm
Lift Distance2-2mm, Lift Speed2-300mm
Notes:
The model is
hollowed
to decrease resin consumption, and
punched
at the bottom
to let resin flow out from model. The wall thickness of hollow part is about
1.8-2.0mm
.
Support parameters:
Density-0.8, attaching point-0.6, lift distance-0.8
Printing parameters:
Exposure time-6000ms, bottom time-80000ms
Layer thickness-50μm, Bottom height-0.3mm
Lift Distance1-2mm, Lift Speed1-48mm
Lift Distance2-2mm, Lift Speed2-300mm
Notes:
The model is tilted about
45°
. The reasons are: 1) the layer has
self-supporting
function when the degree is above 45°; 2) The tilted model
avoids the longest size
paralleled with XY plane to reduce the separation force
. But it will
add the printing
time
due to the height increase. And it needs to add more support at the mouth to
increase adhesion.
Printing parameters:
Exposure time-8000ms, bottom time-80000ms
Layer thickness-50μm, Bottom height-0.3mm
Lift Distance1-2mm, Lift Speed1-48mm
Lift Distance2-2mm, Lift Speed2-300mm
Notes:
The model has many fine characteristics with size about
0.3mm
, so exposure time is
set to
8000ms
to increase the curing hardness.