We’ll now describe s a good practice that minimizes any damage that may occur to all
front panel parts for continued exposure to the soldering iron heat.
It happens often that users not very used to soldering spend too much time on each pad.
An experienced solderer will take 1-2 seconds for each pad, this minimizes the heat the
part is exposed to.
If the solderer takes too much time on each pad the part may heat to a point where the
plastic will start melting/deforming and may render the part useless.
We’ll exemplify the process with jacks.
Step 1 : Start by soldering only one pad of each jack first.
Step 2 : Then solder a second pad of each jack.
Step 3 : Finally solder the remaining pads of all jacks.
Respecting this very simple process for all parts will guarantee no part will be
damaged as they’ll have time to cool down between every soldered pad.