OM-194 199 Page 27
6-14. Troubleshooting – Waviness Of Bead
Waviness Of Bead – weld metal that is not parallel and does not cover
joint formed by base metal.
S-0641
Possible Causes
Corrective Actions
Welding wire extends too far out of nozzle.
Be sure welding wire extends not more than 1/2 in (13 mm) beyond nozzle.
Unsteady hand.
Support hand on solid surface or use two hands.
6-15. Troubleshooting – Distortion
Distortion – contraction of weld metal during welding that forces
base metal to move.
Base metal moves
in the direction of
the weld bead.
S-0642
Possible Causes
Corrective Actions
Excessive heat input.
Use restraint (clamp) to hold base metal in position.
Make tack welds along joint before starting welding operation.
Select lower voltage range and/or reduce wire feed speed.
Increase travel speed.
Weld in small segments and allow cooling between welds.
Содержание 117.205710
Страница 22: ...OM 194 199 Page 19 SECTION 5 ELECTRICAL DIAGRAM SB 186 065 Figure 5 1 Circuit Diagram ...
Страница 38: ...OM 194 199 Page 35 Notes ...
Страница 56: ...OM 194 199 Página 53 SECCION 12 DIAGRAMAS ELECTRICOS SB 186 065 Ilustración 12 1 Diagrama de Circuito ...
Страница 66: ...OM 194 199 Página 63 Apuntes ...
Страница 67: ...OM 194 199 Página 64 ...
Страница 68: ......