B.PROTHERM stainelss steel, heated
– 30 –
Installing the convection heating
module
Convection heating module is disconnected from the mains
Unit door is open
Insert convection heating module into the opening at the unit door and
allow both locking buttons to engage.
Removing areas of corrosion on
stainless steel
New areas of corrosion
Ensure that the power plug is unplugged.
Remove areas of corrosion with a scouring agent or fine sandpaper.
Older/heavier corrosion areas
I
The cleaning measures described here for older and more severe areas
of corrosion are recommendations of the German industry association for
home, heating and kitchen technology (Industrieverband Haus-, Heiz-
und Küchentechnik e. V. (HKI)).
The cleaning measures for older and more severe areas of corrosion may
only be carried out by trained personnel in compliance with the existing
regulations.