17. Click Next. At this point, a different screen will appear depending on the test. If it a creep
test, the Creep screen will appear. If the test is stress rupture, the Creep screen will skip to the
Step Loads screen. See step #21 for the Step Loads screen.
18. The Specimen Loading field specifies how the specimen will be initially loaded once the soak
period has been satisfied. Choose either Multiple steps or Single steps from the pull-down menu.
Typically, multiple steps will be selected.
NOTE: If Plastic Strain is to be separated from Creep data, then the specimen must be loaded in
steps, either manually or via the automatic step load control feature.
19. Select the Minimum Extensometer Classification from the pull-down menu. The system grades
the extensometer to ASTM specifications using a verification process. The system will alert the
operator if the extensometer does not meet the minimum requirements. Select Not Classified to
turn off this feature.
Содержание 2140-M Series
Страница 1: ...WinCCS Lever Arm Tester Series 2140 M 2320 M 2330 M 2330 CC 2410 M 2410 CC...
Страница 2: ...Revised March 2013...
Страница 14: ...14...
Страница 95: ...95 Once these steps are completed the thermocouples will be properly attached to the specimen...
Страница 109: ...109 Appendix C Default Values This appendix includes all the default values typically seen on a WinCCS tester...
Страница 110: ...110...
Страница 111: ...111...
Страница 112: ...112...
Страница 113: ...113...
Страница 115: ...154 East Brook Lane Butler PA 16002 USA 1 724 283 1212 www atspa com...