6.3.4 Report Header
Each report and graph contains a header, which is automatically inserted by the system. Under the
Report Header tab, insert the desired information into the text fields.
6.3.5 Specimen Loading
This section establishes defaults for the loading of stress rupture and creep specimens. The menu is
located under the Specimen Loading tab of the General Setup menu.
Stress Rupture Loading:
ASTM suggests that the preload should be no more than 10 percent of the total
load. Typically, eight is the default value for this section. If the test requires a fixed preload, check the
Use Fixed Preload box and enter the fixed load in pounds into the Preload window. This value may be
changed if necessary when a test is started.
If automatic loading of the specimen is desired once the programmed soak period has expired, check the
Automatically Load box.
Содержание 2140-M Series
Страница 1: ...WinCCS Lever Arm Tester Series 2140 M 2320 M 2330 M 2330 CC 2410 M 2410 CC...
Страница 2: ...Revised March 2013...
Страница 14: ...14...
Страница 95: ...95 Once these steps are completed the thermocouples will be properly attached to the specimen...
Страница 109: ...109 Appendix C Default Values This appendix includes all the default values typically seen on a WinCCS tester...
Страница 110: ...110...
Страница 111: ...111...
Страница 112: ...112...
Страница 113: ...113...
Страница 115: ...154 East Brook Lane Butler PA 16002 USA 1 724 283 1212 www atspa com...