Ceram C0 data sheet
D-4
WILO EMU 3.0
Material needed
- Cleaning agent for cleaning the surface
- Abrasive paper for roughening the surface (select the roughness according to the surface)
- Paintbrush for applying the coating (select the size according to the extent of the damage)
- 2 component coating (Ceram C0 + hardener)
- Vessel for mixing the two components
Working steps
1
Lift the WILO machine from the basin, place it on a secure surface and clean it.
2
Thoroughly clean the damaged area with suitable cleaning agent.
3
Roughen the surface around the damaged area.
4
Mix the 2 component coating (Ceram C0 + hardener) in a 4 to 1 ratio in a suitable vessel.
5
Wait 10 to 15minutes.
6
Apply the finished Ceram C0 coating to the damaged area with a suitable paintbrush. Make
sure the coating is of at least the minimum thickness: 400µm
If you are using a combination of different Ceram types (e.g. C2+C1),
please consult the manufacturer.
7
After repairing the damage, let the Ceram C0 completely dry. See “Hardening time”.
Cleaning tools
Use a commercial solvent (acetone, alcohol or methyl ethyl ketone) to clean your tools immediately
after use. Once the material has dried, it can only be removed by abrasion.
Storage
Store at temperatures between 10°C and 32°C, slight deviations during transport are acceptable.
The containers can be stored unopened for 12 months.
Safety precautions
Before using any products, read the material DIN safety data sheet (MSDS) or the safety regulations
regarding them. Observe all applicable safety regulations when working in enclosed rooms.
Light load
1day
13hours
10hours
Full load
6days
3days
2days
Chemically resistant
10days
6days
4days
Table D-4: Hardening time