12.1.2
Preparing Tungsten for DC Electrode Negative (DCEN) Welding
The electrode should be pointed (tapered) according to the welding current.
Grind end of tungsten on fine grit, hard abrasive wheel before welding. Do not use wheel for other jobs
or tungsten can become contaminated causing lower weld quality.
Rule of thumb is that the taper section should be 2.5 times the Electrode Diameter.
Figure 40
Ideal Tungsten Preparation = Stable ARC
Diameter of the flat left on the end of the Electrode determines amperage capacity.
Figure 41
Wrong Tungsten Preparation = Wandering ARC
Figure 42
Pointing the Tungsten Electrode
The electrode should be pointed according to the welding current.
Figure 43
Electrode Angles
Angle @
Range of Current (Amps)
30°
0 – 30
60-90°
30 -120
90-120°
120 - 250
120°
≥250
Table 12
Summary of Contents for WeldForce WF-140ST
Page 20: ... 20 Weldclass E O E Edition 1 1 2019 05 03 8 4 Primary Schematic Circuit Diagram Figure 13 ...
Page 25: ...WF 140ST WF 180ST Weldclass E O E Edition 1 1 2019 05 03 25 Figure 23 ...
Page 50: ... 50 Weldclass E O E Edition 1 1 2019 05 03 NOTES ...
Page 51: ...WF 140ST WF 180ST Weldclass E O E Edition 1 1 2019 05 03 51 ...
Page 52: ... 52 Weldclass E O E Edition 1 1 2019 05 03 www Weldclass com au ...