6-52
Part curling
Characteristics: Top surface appears rough. Model and support will separate or support and
substrate will separate.
70.
Corrective actions
1.
The part is too dense, try using the “Sparse Fill” option in CatalystEX.
2.
Modeling base has been re-used or is defective. Replace with unused modeling base.
3.
Run Z Calibrations.
4.
Verify proper operation of all chamber fans. Replace fans as needed.
5.
Verify chamber heaters are secured and operating properly. Replace heaters as needed.
6.
Verify X, Y and Z level is within specification. If not level, re-level and calibrate.
Summary of Contents for uPrint
Page 1: ...uPrint and uPrint Plus uPrint SE and uPrint SE Plus Service Manual Part No 209010 0001 Rev D...
Page 11: ...1 2...
Page 35: ...2 24...
Page 179: ...4 132 Figure 4 231 uPrint Plus and uPrint SE Plus measurement points and worksheet BL FL FR BR...
Page 207: ...4 160 Figure 4 275 uPrint and uPrint SE measurement points and worksheet BL FL FR BR...
Page 267: ...5 58...
Page 343: ...6 76...
Page 359: ...7 16...
Page 373: ...8 14...