overlapped. The overlap width is 100mm.
5). After temperature and speed have been determined, insert material to be welded between the
two pressure rollers, make machine body parallel with edges of base materials and engage press lever
handle for proper motion. Generally, only observation of deviation between welding mark and base
materials is needed for operator, and timely make correction on small degree.
6). When welding will be ended, timely press lever handle to disengage upper and lower pressure
roller to prevent rubber wheel damage for long duration.
7). Excessive temperature high and low may occur because of thermal inertia. On this condition,
temperature deviation may be compensated by speed regulation on a small degree.
8). A “T” shape overlap is formed between welded material and another material. Welding method is
shown as fig.5, tightly butt the overlap head of hot wedge against weld mark, and beveling cut length is
approximately 100mm.
Fig.5“T”shape welding diagram
6. Replacement of components
1). Replacement of hot wedge assembly
Remove the front end covering, remove the 4-M4 screws and tapping screw, remove a half housing,
release 4-M3 screws, remove the 2-M5 screws that connect heating support and slide carriage, remove
hot wedge and replace with a new one, and reassemble the complete machine (shown as fig.6). Note:
conform to color on wiring.
(Refer to fig.10 and text information)