ENERSYS Ltd, NEWPORT
COMPONENT MAINTENANCE MANUAL
LEARJET PART NO.7624308001-003
ELN PART NO.9750R0824-Rev04
If three consecutive half-hourly voltage readings show a voltage
decrease, the charge may be discontinued.
After charging, rest the battery for 4 Hours.
(2)
Constant
Voltage
Charge at 29.0 volts (minimum of 10 Amps available) for 4 Hours
After charging, rest the battery for 4 Hours.
F.
Discharge Test Procedure
Discharging should be conducted between 20°C (68°F) and 30°C(86°F).
Discharge at 10 Amps to 20 Volts or for 48 Minutes, whichever occurs
soonest.
G.
Commissioning
Procedure
(1)
Visually inspect the exterior of the battery casing for signs of damage,
cracks,
corrosion,
etc.
(2)
Examine the battery terminal connector for signs of corrosion, damage
and water/dirt ingress; clean if necessary.
(3)
Check open circuit voltage, if the open circuit voltage is in excess of or
equal to 25.5 volts, ensure that the battery is clean and issue for
service.
(4)
If the open circuit voltage is above or equal to 25.3 volts but below
25.5 volts, charge in accordance with section 4.E. After resting the
battery for 4 Hours, ensure that the battery is clean and issue for
service.
Page 106
24-01-03
Apr 21/99